石嘴山市成套鎂陽極 出廠自帶帶3米線鎂陽極
犧牲陽極電化學(xué)性能測(cè)試實(shí)驗(yàn)裝置由直流數(shù)字恒壓源、輔助陰極、參比電極、高阻抗數(shù)字萬
用表、實(shí)驗(yàn)容器組成,裝置如圖1所示。采用WLS型恒壓源為測(cè)試過程提供電源,電壓控制精度0.1V
。輔助陰極采用鍍鋅圓筒,內(nèi)外面均為工作面,總面積840cm
2。以飽和甘汞電極(SCE)
做為參比電極,采用高阻抗數(shù)字萬用表測(cè)量犧牲陽極電位。實(shí)驗(yàn)容器采用容積為2L
的燒杯,使得犧牲陽極試樣和輔助陰極*浸沒在試驗(yàn)溶液中,電量通過銅電量計(jì)測(cè)量,電流通過數(shù)萬用表監(jiān)測(cè),實(shí)驗(yàn)介質(zhì)采用
GB/T 17848-1999
要求的人造海水
鎂合金的防腐蝕方法
鎂合金防腐蝕的方法主要有四種,分別是:化學(xué)轉(zhuǎn)化處置、陽極氧化、金屬涂層、激光處置。
化學(xué)轉(zhuǎn)化處理
鎂合金的化學(xué)轉(zhuǎn)化膜按溶液可分為:鉻酸鹽系、有機(jī)酸系、磷酸鹽系、KMnO4系、稀土元素系和錫酸鹽系等。
傳統(tǒng)的鉻酸鹽膜以The structure of Cr is compact, and Cr with structural water has good self repairing function, and its corrosion resistance is very strong. But Cr has great toxicity, and the cost of wastewater treatment is higher. It is imperative to develop chrome free conversion process. The chemical conversion film of amorphous structure can be obtained by the treatment of magnesium alloy in KMnO4 solution. The corrosion resistance of magnesium alloy is similar to that of chromate film.堿性錫酸鹽的化學(xué)轉(zhuǎn)化處理可作為鎂合金化學(xué)鍍鎳的前處理,取代傳統(tǒng)的含Cr、F或CN等有害離子的工藝?;瘜W(xué)轉(zhuǎn)化膜多孔的結(jié)構(gòu)在鍍前的活化中表現(xiàn)出很好的吸附性,并能改鍍鎳層的結(jié)合力與耐蝕性。wz75462226
有機(jī)酸系處理所獲得的轉(zhuǎn)化膜能同時(shí)具備腐蝕保護(hù)和光學(xué)、電子學(xué)等綜合性能,在化學(xué)轉(zhuǎn)化處理的新發(fā)展中占有很重要的地位。
化學(xué)轉(zhuǎn)化膜較薄、軟,防護(hù)能力弱,一般只用作裝飾或防護(hù)層中間層。
陽極氧化
陽極氧化可得到比化學(xué)轉(zhuǎn)化更好的耐磨損、耐腐蝕的涂料基底涂層,并兼有良好的結(jié)合力、電絕緣性和耐熱沖擊等性能,是鎂合金常用的表面處理技術(shù)之一。
傳統(tǒng)鎂合金陽極氧化的電解液一般都含鉻、氟、磷等元素,不僅污染環(huán)境,也損害人類健康。近年來研究開發(fā)的環(huán)保型工藝所獲得的氧化膜耐腐蝕等性能較經(jīng)典工藝Dow17和HAE有大程度的提高。優(yōu)良的耐蝕性來源于陽極氧化后Al、Si等元素在其表面均勻分布,使形成的氧化膜有很好的致密性和完整性。
一般認(rèn)為氧化膜中存在的孔隙是影響鎂合金耐蝕性能的主要因素。研究發(fā)現(xiàn)通過向陽極氧化溶液中加入適量的硅-鋁溶膠成分,一定程度上能改善氧化膜層厚度、致密度,降低孔隙率。而且溶膠成分會(huì)使成膜速度出現(xiàn)階段性快速和緩慢增長(zhǎng),但基本上不影響膜層的X射線衍射相結(jié)構(gòu)。
但陽極氧化膜的脆性較大、多孔,在復(fù)雜工件上難以得到均勻的氧化膜層。wz75462226